Specifications
HOME > Specifications > Material
Material
Material | |||||||||||||
Name | JIS | ASTM | Material no. | Working Temp | Tensile Strength | E-modulus in KN//mm² | Thickness range | ||||||
°C | N/mm² | RT °C | 100°C | 200°C | 300 °C | 400°C | 500°C | 600°C | mm | ||||
Spring Steel | |||||||||||||
T8A | SK5 | – | 1.183 | – 50 to +100 | 1200-1800 | 206 | 202 | 0.1 to 3.5 | |||||
50CrV4 | SUP10 | 6150 | 1.8159 | – 50 to +200 | 1200-1800 | 206 | 202 | 196 | - | - | - | - | 0.3 to 30 |
C75 | – | 1074 | 1.0773 | – 50 to +100 | 1200-1800 | 206 | 202 | - | - | - | - | - | 0.3 to 30 |
60Si2Mn | SUP6 | 9260 | 1.0906 | – 50 to +200 | 1200-1800 | 206 | 202 | 196 | - | - | - | - | 0.3 to 30 |
Corrosion Resistant Steel | |||||||||||||
X 10CrNi 18-8 | SUS301 | 301 | 1.431 | – 200 to +200 | 1150-1500 | 190 | 186 | 180 | - | - | - | - | 0.2 to 4.0 |
X 5CrNi 18-10 | SUS304 | 304 | 1.4301 | – 200 to +200 | 1000-1500 | 185 | 179 | 171 | - | - | - | - | 0.2 to 4.0 |
X 5CrNiMo 17-12-2 | SUS316 | 316 | 1.4401 | – 200 to +200 | 1000-1500 | 180 | 176 | 171 | - | - | - | - | 0.2 to 3.5 |
X 7CrNiAl 17-7 | SUS631 | 17-7PH | 1.4568 | – 200 to +300 | 1150-1700 | 195 | 190 | 180 | 171 | - | - | - | 0.2 to 9.0 |
X5CrNiCuNb 16-4 | SUS630 | 17-4PH | 1.4542 | – 200 to +300 | 1150-1700 | 195 | 190 | 180 | 171 | - | - | - | 0.2 to 9.0 |
X8CrNiMoAl 15-7-2 | 15-7Mo | 1.4532 | – 200 to +300 | 1150-1700 | 195 | 190 | 180 | 171 | - | - | - | 0.2 to 9.0 | |
Thermally Stable Steel | |||||||||||||
X39CrMo 17-1 | – | - | 1.4122 | – 50 to +400 | 1200-1400 | 215 | 212 | 205 | 200 | 190 | - | - | 0.3 to 30 |
X 22CrMoV 12-1 | – | - | 1.4923 | – 50 to 500 | 1200-1400 | 216 | 209 | 200 | 190 | 179 | 167 | - | 1.5 to 20 |
X 30WCrV53 | SKD4 | – | 1.4923 | – 50 to 500 | ≥1470 | 216 | 209 | 200 | 190 | 179 | 167 | – | 1.5 to 20 |
Tool Steel | |||||||||||||
X40CrMoV5-1 | SKD61 | H13 | 1.2344 | – 150 to 600 | 1650-1990 | 206 | 200 | 186 | 196 | 189 | 158 | - | 0.3 to 30 |
Antimagnetic and Corrosion Resistant Steel | |||||||||||||
CuSn 8 | C5210 | - | 2.103 | – 50 to +100 | 590-690 | 115 | 110 | - | - | - | - | - | 0.1 to 6.0 |
CuBe 2 | C1720 | - | 2.1247 | – 260 to +200 | 1270-1450 | 135 | 131 | 125 | - | - | - | - | 0.1 to 2.5 |
Nickel and Cobalt Alloys Steel | |||||||||||||
Inconel X750 | – | 5542L | 2.4669 | – 200 to +600 | ≥ 1170 | 214 | 207 | 198 | 190 | 179 | 170 | 158 | 0.1 to 7.0 |
Inconel X718 | – | 5596J | 2.4668 | – 200 to +600 | ≥ 1240 | 199 | 195 | 190 | 185 | 179 | 174 | 167 | 0.1 to 7.0 |
Nimonic 90 | – | 5829C | 2.4632 | – 200 to +700 | ≥ 1100 | 220 | 216 | 208 | 202 | 193 | 187 | 178 | 0.1 to 7.0 |